基于有限元的含腐蚀缺陷原油集输管道剩余强度研究*
分享到:

《中国安全生产科学技术》[ISSN:1673-193X/CN:11-5335/TB]

卷:
17
期数:
2021年10期
页码:
127-132
栏目:
职业安全卫生管理与技术
出版日期:
2021-10-31

文章信息/Info

Title:
Study on residual strength of crude oil gathering and transportation pipeline containing corrosion defects based on finite element
文章编号:
1673-193X(2021)-10-0127-06
作者:
何雨珂孔令圳王金鑫王大文刘正
(1.西南石油大学 石油与天然气工程学院,四川 成都 610500;
2.延长油田股份有限公司,陕西 延安 716000)
Author(s):
HE Yuke KONG Lingzhen WANG Jinxin WANG Dawen LIU Zheng
(1.School of Petroleum Engineering,Southwest Petroleum University,Chengdu Sichuan 610500,China;
2.Yanchang Oilfield Co.,Ltd.,Yan’an Shaanxi 716000,China)
关键词:
集输管道ABAQUS均匀腐蚀缺陷剩余强度评价
Keywords:
gathering and transportation pipeline ABAQUS uniform corrosion defect residual strength evaluation
分类号:
X937
DOI:
10.11731/j.issn.1673-193x.2021.10.019
文献标志码:
A
摘要:
为研究含腐蚀缺陷原油集输管道的剩余强度,以延长油田集输系统常用的20#管线钢为例,采用ABAQUS建立1/2腐蚀管道有限元模型,研究单个均匀腐蚀缺陷对集输管道剩余强度的影响,分析缺陷位置、缺陷长度、缺陷宽度和缺陷深度的影响规律,并采用Matlab对缺陷长度和缺陷宽度角的模拟结果进行拟合,拟合确定系数R2均达99.0%以上。结果表明:集输管道的剩余强度受缺陷位置的影响较小;随着缺陷长度的增加先减小后保持不变,随着缺陷宽度的增加先略微增加后保持不变,建立缺陷深度分别为1.5,2.0,2.5 mm的有限元模型,得到缺陷临界长度分别为210,140,130 mm,缺陷宽度角分别为56°,57°,141°;剩余强度受缺陷深度的影响最大,会随着缺陷深度的增加而减小;缺陷深度越大,缺陷长度和缺陷宽度对剩余强度的影响越大。
Abstract:
In order to study the residual strength of crude oil gathering and transportation pipelines containing the corrosion defects,taking the 20# pipeline steel commonly used in the gathering and transportation system of Yanchang oilfield as an example,a finite element model of 1/2 corrosion pipeline was established by using ABAQUS,and the influence of single uniform corrosion defect on the residual strength of gathering and transportation pipeline was studied.The influence laws of defect location,defect length,defect width and defect depth were analyzed,then the fitting on the simulation results of defect length and defect width angle was conducted by using Matlab,and all the fitting determination coefficient R2 reached more than 99.0%.The results showed that the residual strength of the gathering and transportation pipeline was less affected by the defect location.With the increase of defect length,it decreased first and then remained unchanged.With the increase of defect width,it slightly increased first and then remained unchanged.The finite element models with the defect depth of 1.5 mm,2.0 mm and 2.5 mm respectively were established,the critical lengths of defect were 210 mm,140 mm and 130 mm,respectively,and the defect width angles were 56°,57° and 141°,respectively.The residual strength was most affected by the defect depth,and it decreased with the increase of defect depth.The greater the defect depth,the greater the influence of defect length and defect width on the residual strength.

参考文献/References:

[1]张照鸿.延长气田集输管道的事故分析及风险评价[D].西安:西安石油大学,2014.
[2]李涛,贺磊.陆上油田集输管道腐蚀失效管理与可靠性研究[J].化工管理,2020(15):219-220. LI Tao,HE Lei.Research on corrosion failure management and reliability of onshore oil field gathering pipeline[J].Chemical Enterprise Management,2020(15):219-220.
[3]黄坤,吴佳丽,全恺,等.含腐蚀缺陷油气管道评价技术研究进展[J].表面技术,2018,47(1):116-122. HUANG Kun,WU Jiali,QUAN Kai,et al.A review on evaluation technology of oil-gas pipelines with corrosion defect[J].Surface Technology,2018,47(1):116-122.
[4]王增国,刚蓓,郑莉,等.含体积型缺陷管道剩余强度评价方法研究[J].科学技术创新,2020(30):20-21. WANG Zengguo,GANG Bei,ZHENG Li,et al.Study on residual strength evaluation method of pipeline with volumetric defect[J].Scientific and Technological Innovation,2020(30):20-21.
[5]HOANG V T,龙伟,刘华国,等.基于有限元的含均匀腐蚀缺陷油气管道剩余强度[J].油气储运,2018,37(2):157-161. HOANG V T,LONG Wei,LIU Huaguo,et al.Research on residual strength of metallic oil and gas pipelines with uniform corrosion defects based on finite element method[J].Oil & Gas Storage and Transportation,2018,37(2):157-161.
[6]THIBANKUMAR A,SARAVANAN K,MARK O.Residual strength analysis of pipeline with circumferential groove corrosion subjected to internal pressure[J].Materials Today:Proceedings,2020,29(10):88-93.
[7]张足斌,王婷婷,焦震.含体积型缺陷管道的剩余强度分析[J].油气田地面工程,2019,38(10):105-109,117. ZHANG Zubin,WANG Tingting,JIAO Zhen.Residual strength analysis of pipeline with volumetric defects[J].Oil-Gas Field Surface Engineering,2019,38(10):105-109,117.
[8]CHANYALEW T B,CHE I M,SARAVANAN K.Strength assessment of a corroded pipeline through the burst test:case study[J].Journal Of Pipeline Systems Engineering and Practice,2016,7(3):04016003.
[9]马廷霞,潘玉林,黄文,等.含等壁厚体积型缺陷油气管道的剩余强度评价[J].材料保护,2020,53(5):34-41. MA Tingxia,PAN Yulin,HUANG Wen,et al.Residual strength evaluation of oil and gas pipeline with volumetric defects of the same thickness[J].Materials Protection,2020,53(5):34-41.
[10]王秋妍,顾晓婷,吴毅琦,等.X100钢管腐蚀剩余强度评价方法研究[J].钢结构,2017,32(3):113-116. WANG Qiuyan,GU Xiaoting,WU Yiqi,et al.Research on evaluation method of residual strength of corroded X100 pipeline[J].Steel Construction,2017,32(3):113-116.
[11]崔凯燕,王晓霖,杨文,等.基于内检测评价的管道安全维修决策[J].中国安全科学学报,2019,29(2):172-177. CUI Kaiyan,WANG Xiaolin,YANG Wen,et al.ILI assessment based policy-making on pipeline safety maintenance[J].China Safety Science Journal,2019,29(2):172-177.
[12]吕若飞.基于有限元法的埋地钢质管道的剩余强度研究[D].北京:中国地质大学(北京),2019.
[13]王战辉,马向荣,高勇,等.不同钢级油气管道剩余强度评价方法对比[J].材料保护,2020,53(1):67-74. WANG Zhanhui,MA Xiangrong,GAO Yong,et al.Comparison of residual strength evaluation methods for different grades of oil and gas pipelines[J].Materials Protection,2020,53(1):67-74.
[14]孙明明,李昕,刘锦昆.基于应变强化效应的管道流变应力分析[J].哈尔滨工程大学学报,2021,42(1):89-95. SUN Mingming,LI Xin,LIU Jinkun.Flow-stress analysis of a steel pipeline considering the strain-hardening effect[J].Journal of Harbin Engineering University,2021,42(1):89-95.
[15]帅义,帅健,狄彦.含凹陷管道全尺寸爆破试验[J].油气储运,2017,36(1):44-48. SHUAI Yi,SHUAI Jian,DI Yan.Full-scale burst experiments on dented pipeline[J].Oil & Gas Storage and Transportation,2017,36(1):44-48.

相似文献/References:

[1]廖柠,黄坤,吴锦,等.基于ABAQUS的穿越公路输气管道力学性状分析[J].中国安全生产科学技术,2017,13(5):61.[doi:10.11731/j.issn.1673-193x.2017.05.010]
 LIAO Ning,HUANG Kun,WU Jin,et al.Analysis on mechanical properties of gas pipeline crossing highway based on ABAQUS[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2017,13(10):61.[doi:10.11731/j.issn.1673-193x.2017.05.010]
[2]王宝迪,宿利平,刘洋.改进西原蠕变模型研究及二次开发计算*[J].中国安全生产科学技术,2022,18(8):128.[doi:10.11731/j.issn.1673-193x.2022.08.019]
 WANG Baodi,SU Liping,LIU Yang.Improved Nishihara creep model research and secondary development calculation[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2022,18(10):128.[doi:10.11731/j.issn.1673-193x.2022.08.019]

备注/Memo

备注/Memo:
收稿日期: 2021-04-18
* 基金项目: 延长油田股份有限公司委托科技项目(Ycsy2019ky-C-5-8);四川省科技计划项目(No.2019YJ0400)
作者简介: 何雨珂,硕士研究生,主要研究方向为油气管道完整性评价。
更新日期/Last Update: 2021-11-03