Title:
Analysis on erosion wear effect of fracturing manifold elbow in shale gas
文章编号:
1673-193X(2020)-10-0053-06
作者:
周兰张红陈文康冯定张羽
(1.长江大学 机械工程学院,湖北 荆州 434023;
2.湖北省油气钻完井工具工程技术研究中心,湖北 荆州 434023;
3.中石化石油机械股份有限公司第四机械厂,湖北 荆州 434020)
Author(s):
ZHOU Lan ZHANG Hong CHEN Wenkang FENG Ding ZHANG Yu
(1.School of Mechanical Engineering,Yangtze University,Jingzhou Hubei 434023,China;
2.Hubei Engineering Research Center for Oil and Gas Drilling and Completion Tools,Jingzhou Hubei 434023,China;
3.Fourth Machinery Factory of SINOPEC Petroleum Machinery Co.,Ltd.,Jingzhou Hubei 434020,China)
关键词:
高压管汇弯头冲蚀磨损
Keywords:
high pressure manifold elbow erosion wear
分类号:
X937
DOI:
10.11731/j.issn.1673-193x.2020.10.008
文献标志码:
A
摘要:
为减小管汇弯头所受的冲蚀磨损率,在考虑固液两相流模型、流体控制方程及冲蚀磨损计算模型基础上,建立高压弯头冲蚀磨损数值模型,以现场工况为依据,对压裂液的流动速度、压裂液黏度、质量流量以及颗粒直径进行控制调整,研究高压弯头的冲蚀因素,得出各因素对弯头冲蚀磨损机理,总结各因素对弯头冲蚀磨损规律。结果表明:为减小冲蚀磨损率,提高高压弯头使用寿命,应减小施工压裂液的质量流量、选用直径较小的颗粒、压裂液黏度应为0.014 Pa·s左右;针对高压弯头提出弯径比为2~3、适当增加弯头的壁厚等改进措施。
Abstract:
In order to reduce the erosion wear rate of manifold elbow,based on the solidliquid twophase flow model,fluid control equations and erosion wear calculation model,the erosion wear numerical model of highpressure elbow was established.Based on the field conditions,the flow velocity,fracturing fluid viscosity,mass flow rate and solid particle diameter of the fracturing fluid were controlled and adjusted.After that,by studying the erosion factors of the highpressure elbow,the erosion wear mechanism and law of each factor to the elbow were obtained.The results showed that in order to reduce the erosion wear rate and improve the service life of highpressure elbow,it was suggested to reduce the mass flow rate of constructing fracturing fluid,select the solid particles with smaller diameter and the fracturing fluid viscosity of about 0.014 Pa·s.In addition,the improvement measures such as controlling the bending diameter ratio between 2~3 and appropriately increasing the wall thickness of elbow were put forward for the high pressure elbow.

参考文献/References:

[1]刘寒月,魏宁.固体颗粒对油气井管柱的冲蚀损伤研究[J].中国矿业,2018,27(2):157-162. LIU Hanyue,WEI Ning.Study on erosion damage of oil and gas well string by solid particles [J].China Mining,2018,27(2):157-162.
[2]李方淼,李美求,宋杨,等.液固两相流对活动弯头的冲蚀研究[J].石油机械,2019,47(10):107-111. LI Fangmiao,LI Meiqiu,SONG Yang,et al.Erosion of liquid-soild two-phase flow on bend pipe union [J].China Petroleum Machinery,2019,47(10):107-111.
[3]冯定,陈文康,孙巧雷,等.组合油管对水平井修井管柱下入能力的影响研究[J].工程设计学报,2020,27(1):51-58. FENG Ding,CHEN Wenkang,SUN Qiaolei,et al.Study on the influence of combined tubing on running capacity of workover string in horizontal well [J].Chinese Journal of Engineering Design,2020,27(1):51-58.
[4]ALDO I,MATTHEW T S,WILLIAM M D.A computational fluid dynamics model to evaluate the inlet stroke performance of a positive displacement reciprocating plunger pump[J].Power and Energy,2014,228(5):574-584.
[5]JI B,PENG X X,WU Y L,et al.Unsteady numerical simulation of cavitation turbulence flow around a highly skewed model marine propeller [J].ASME Journal of Fluids Engineering,2011,133(1):011102.
[6]祝效华,曾云义,陈波,等.考虑流固耦合的双弯头压裂管汇的振动特性[J].天然气工业,2018,38(1):95-101. ZHU Xiaohua,ZENG Yunyi,CHEN Bo,et al.Vibration characteristics of double-elbow fracturing manifold considering fluid-solid interaction [J].Natural Gas Industry,2018,38(1):95-101.
[7]赵钰,王鹏,许凤华,等.钻井用水力振荡器阀组压降计算方法[J].科学技术与工程,2018,18(15):94-98. ZHAO Yu,WANG Peng,XU Fenghua,et al.Methods for calculation of pressure drop of the valve section of the drilling hydraulic oscillator [J].Science Technology and Engineering,2018,18(15):94-98.
[8]赵钰,龚盼,刘志刚,等.新型射流振荡器工作原理与试验研究[J].流体机械,2018,46(9):13-17,83. ZHAO Yu,GONG Pan,LIU Zhigang,et al.Working principle and experimental research of a new type fluidic oscillator [J].Fluid Machinery,2018,46(9):13-17,83.
[9]胡成,邓福成,杨永刚,等.基于正交试验的割缝筛管冲蚀磨损分析[J].石油机械,2020,48(1):149-154. HU Cheng,DENG Fucheng,YANG Yonggang,et al.Analysis on erosion wear of slotted screen tube based on orthogonal test [J].China Petroleum Machinery,2020,48(1):149-154.
[10]向正新,李思行,钱利勤,等.压裂球座冲蚀磨损规律研究和结构优化[J].工程设计学报,2017,24(5):555-562. XIANG Zhengxin,LI Sixing,QIAN Liqin,et al.Research on erosion wear law and structure optimization of fracturing ball seat [J].Journal of Engineering Design,2017,24(5):555-562.
[11]吴晗,刘少胡,刘旭辉,等.焊肉位置对连续管冲蚀磨损规律研究[J].中国安全生产科学技术,2017,13(2):138-142. WU Han,LIU Shaohu,LIU Xuhui,et al.Study on the erosion and abrasion law of continuous pipe by welding meat position [J].Journal of Safety Science and Technology,2017,13(2):138-142.
[12]HATTORI S,KISHIM O M.Prediction of cavitation erosion on stainless steel components in centrifugal pumps [J].Wear,2008,265(11-12):1870-1874.
[13]成芳,易先中,彭灼,等.页岩气压裂弯管中液固两相流冲蚀磨损的数值模拟[J].中国安全生产科学技术,2019,15(11):29-35. CHENG Fang,YI Xianzhong,PENG Zhuo,et al.Numerical simulation of liquid-solid two-phase flow erosion and wear in shale gas fracturing elbow [J].Journal of Safety Science and Technology,2019,15(11):29-35.
[14]黄坤,邓平,李岳鹏,等.气固两相流90°弯管抗冲蚀结构优化[J].中国安全生产科学技术,2019,15(8):94-100. HUANG Kun,DENG Ping,LI Yuepeng,et al.Optimization of erosion resistant structure of 90 ° elbow for gas-solid two-phase flow [J].Journal of Safety Science and Technology,2019,15 (8):94-100.
[15]刘洪亮,李美求,潘力,等.压裂工况下T形三通冲蚀影响数值模拟[J].科学技术与工程,2020,20(10):3893-3897. LIU Hongliang,LI Meiqiu,PAN Li,et al.Numerical simulation of T-shaped three-way erosion effect under fracturing conditions [J].Science Technology and Engineering,2020,20(10):3893-3897.

相似文献/References:

[1]杨帆,李雷雷,姜文全,等.埋地热油管道泄漏裂纹开裂的应力研究[J].中国安全生产科学技术,2015,11(6):63.[doi:10.11731/j.issn.1673-193x.2015.06.010]
 YANG Fan,LI Lei-lei,JIANG Wen-quan,et al.Study on stress of crack initiation in leakage of buried hot oil pipeline[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2015,11(10):63.[doi:10.11731/j.issn.1673-193x.2015.06.010]
[2]刘洪斌,牟浩.加砂压裂中固体支撑剂对压裂管道的冲蚀磨损研究[J].中国安全生产科学技术,2018,14(1):87.[doi:10.11731/j.issn.1673-193x.2018.01.014]
 LIU Hongbin,MU Hao.Study on erosion wear of fracturing pipe caused by solid proppant in sand fracturing[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2018,14(10):87.[doi:10.11731/j.issn.1673-193x.2018.01.014]
[3]王彦然,樊建春,杨思齐,等.高压管汇磁致伸缩导波缺陷检测模拟研究[J].中国安全生产科学技术,2020,16(3):18.[doi:10.11731/j.issn.1673-193x.2020.03.003]
 WANG Yanran,FAN Jianchun,YANG Siqi,et al.Simulation study on detection of magnetostrictive guided wave defects in highpressure manifold[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2020,16(10):18.[doi:10.11731/j.issn.1673-193x.2020.03.003]

备注/Memo

备注/Memo:
收稿日期: 2020-06-17
* 基金项目: 国家自然科学基金项目(51704034);国家重大专项课题项目(2016ZX05038-002-LH001);中海石油(中国)有限公司湛江分公司横向项目(CCL2017ZJFN2272)
作者简介: 周兰,硕士研究生,主要研究方向为管柱力学。
通信作者: 冯定,博士,教授,主要研究方向为石油机械及井下工具设计、管柱力学。
更新日期/Last Update: 2020-11-21