[1]陈晓坤,陈言,王伟峰,等.单芯铜线过电流故障电弧熔痕的微观特征研究*[J].中国安全生产科学技术,2020,16(12):136-142.[doi:10.11731/j.issn.1673-193x.2020.12.022]
 CHEN Xiaokun,CHEN Yan,WANG Weifeng,et al.Study on microcosmic characteristics of arc melting trace caused by overcurrent fault of singlecore copper wire[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2020,16(12):136-142.[doi:10.11731/j.issn.1673-193x.2020.12.022]
点击复制

单芯铜线过电流故障电弧熔痕的微观特征研究*
分享到:

《中国安全生产科学技术》[ISSN:1673-193X/CN:11-5335/TB]

卷:
16
期数:
2020年12期
页码:
136-142
栏目:
职业安全卫生管理与技术
出版日期:
2020-12-31

文章信息/Info

Title:
Study on microcosmic characteristics of arc melting trace caused by overcurrent fault of singlecore copper wire
文章编号:
1673-193X(2020)-12-0136-07
作者:
陈晓坤陈言王伟峰徐学岩李阳张安邦杨雯
(1.西安科技大学 安全科学与工程学院,陕西 西安 710054;
2.中国人民警察大学 消防工程系,河北 廊坊 065000)
Author(s):
CHEN Xiaokun CHEN Yan WANG Weifeng XU Xueyan LI Yang ZHANG Anbang YANG Wen
(1.College of Safety Science and Engineering,Xi’an University of Science and Technology,Xi’an Shaanxi 710054,China;
2.College of Fire Protection Engineering,Chinese People’s Police University,Langfang Hebei 065000,China)
关键词:
火灾调查过电流故障电弧熔痕金相组织铜导线
Keywords:
fire investigation overcurrent fault arc melting trace metallographic structure copper wire
分类号:
X928.7
DOI:
10.11731/j.issn.1673-193x.2020.12.022
文献标志码:
A
摘要:
为准确认定电气火灾中过电流故障,模拟4~7倍额定电流(Ie)条件下单芯铜导线过电流故障,利用光学显微镜和扫描电子显微镜(SEM)分析过电流故障电弧熔痕的组织特征,并结合Image-Pro Plus软件测定晶粒直径、周长和面积,探究金相组织的量化判据和变化规律。结果表明:当I=4Ie时,过电流故障电弧熔痕的金相组织主要为方向性较强的树枝晶;当I=5Ie,6Ie时,金相组织内树枝晶占比减小,胞状晶占比升高;当I=7Ie时,方向性较弱的胞状晶占主导。随着电流增加,晶粒的平均直径、周长和面积均呈增长趋势。通过火灾案例分析可知,实验结果与现场的电弧熔痕组织特征基本相符,验证火灾事故原因为过电流故障。
Abstract:
In order to accurately identify the overcurrent faults in the electrical fires,the overcurrent faults of singlecore copper wire under the conditions of 4~7 times rated current (Ie) were simulated.The optical microscopy and scanning electron microscopy (SEM) were used to analyze the structural characteristics of arc melting trace caused by the overcurrent fault,and the ImagePro Plus software was used to determine the grain diameter,circumference and area,then the quantitative criteria and changing laws of metallographic structure were explored.The results showed that when I=4Ie,the metallographic structure of arc melting trace caused by overcurrent faults was mainly the dendrites with stronger directivity.When I=5Ie or 6Ie,the proportion of dendrites in the metallographic structure decreased,while the proportion of cellular crystals increased.When I=7Ie,the cellular crystal with weaker directivity was dominated.As the current increased,the average diameter,circumference and area of the grains increased.Through the fire case analysis,it was found that the experimental results were basically consistent with the structure characteristics of onsite arc melting trace,and the fire accident was verified to be caused by overcurrent fault.

参考文献/References:

[1]BABRAUSKAS V.How do electrical wiring faults lead to structure ignitions[J].Fire and Arson Investigator,2002,52:39-45.
[2]FUJITA O,KYONO T,KIDO Y,et al.Ignition of electrical wire insulation with short-term excess electric current in microgravity[J].Proceeding of the Combustion Institute,2011,33(2):2617-2623.
[3]BABRAUSKAS V.Arc mapping:a critical review[J].Fire Technology,2018,54(3):749-780.
[4]National Fire Protection Association.NFPA921 guide for fire and explosion investigations 2017 edition[M].America:Standards Council,2017.
[5]SOULINARIS G K,HALEVIDIS C D,POLYKRATI A D,et al.Evaluation of the thermal stresses and dielectric phenomena in the investigation of the causes of wildfire involving distribution power lines[J].Electric Power Systems Research,2014,117(5):76-83.
[6]BABRAUSKAS V.Fire due to electric arcing:can ‘cause’ beads be distinguished from ‘victim’ beads by physical or chemical testing[J].Fire and Materials,2003,36(8):189-201.
[7]WRIGHT S A,LOUD J D,BLANCHARD R A.Globules and beads:what do they indicate about small-diameter copper conductors that have been through a fire[J].Fire Technology,2015,51(5):1051-1070.
[8]XIE D B,WANG W,LYU S,et al.Visual and oxide analysis for identification of electrical fire scene[J].Forensic Science International,2018,285(5):21-24.
[9]GU H X,XUE L,ZHANG Y F,et al.Analysis on micro-regional characters of the resistance wires surface in electrical immersion heater by SEM/EDX[J].Forensic Science International,2014,238(24):96-100.
[10]TAKAKI A.On the effect of thermal histories upon the metallographic structure of electric wires[J].National Research Institute of Police Science,1971,24(2):48-56.
[11]KUAN H L,YUNG H S,GUO J C,et al.Microstructural study on molten marks of fire-causing copper wires[J].Materials,2015,8(6):3776-3790.
[12]BABRAUSKAS V.Research on electrical fires:the state of the art[J].Fire Safety Science,2008,9(6):3-18.
[13]GAO A,ZHAO C Z,XU F,et al.Fire risk and failure mechanism of copper wire under overcurrent fault condition[J].Procedia Engineering,2013,52(8):119-123.
[14]何豪.通电聚乙烯导线火蔓延伴随的熔融滴落行为研究[D].合肥:中国科学技术大学,2017.
[15]ASTM International.Standard practice for preparation of metallographic specimens1:ASTM E 3—2017 [S].American:American Society for Testing and Materials,2017.
[16]ASTM International.Standard practice for macroetching metals and Alloys1:ASTM E 407—2007 [S].American:American Society for Testing and Materials,2007.
[17]KOTHANDARAMAN C P.Fundamentals of heat and mass transfer[M].Coimbatore Wiley:New Age International,2001.
[18]吴细秀.开关电器触头材料喷溅侵蚀模型研究及其试验[D].武汉:华中科技大学,2005.
[19]HURLEY M J,GOTTUK D T,JOHN R H,et al.SFPE Handbook of fire protection engineering[M].New York:Society of Fire Protection Engineers,2016.
[20]CHOUDHURY A,REUTHER K,WESNER E,et al.Comparison of phase-field and cellular automa-ton models for dendritic solidification in Al-Cu alloy[J].Computational Materials Science,2012,55(6):263-268.
[21]TENG J,LIU S,TRIVEDI R.Onset of sidewise instability and cell-dendrite transition in directional solidification[J].Acta Materialia,2009,57(12):3497-3508.
[22]KURZ W,FISHER D J.Dendrite growth at the limit of stability:tip radius and spacing[J].Acta Metallurgica,1981,29(1):11-20.
[23]LUDWIG A.Comparison of dendrites of a pure material with thermal alloy dendrites:an experimental method to estimate the t0-temperature[J].Acta Materialia,2001,49(1):165-168.
[24]SPAEPEN F.A structural model for the solid-liquid interface in monatomic systems[J].Acta Metallurgica,1975,23(6):729-743.

相似文献/References:

[1]王冠宁,陈涛,邢菲,等.监控完全遮挡场景下火焰特征分析方法*[J].中国安全生产科学技术,2021,17(9):13.[doi:10.11731/j.issn.1673-193x.2021.09.002]
 WANG Guanning,CHEN Tao,XING Fei,et al.Analysis method of flame characteristic in scene of completely blocked surveillance[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2021,17(12):13.[doi:10.11731/j.issn.1673-193x.2021.09.002]
[2]姜文宇,吴坚,孙烨,等.过电流故障铝导线熔痕部位与组织特征关联性研究*[J].中国安全生产科学技术,2022,18(1):75.[doi:10.11731/j.issn.1673-193x.2022.01.012]
 JIANG Wenyu,WU Jian,SUN Ye,et al.Study on correlation between location of melted marks and microstructure characteristics of aluminum conductor under overcurrent fault[J].JOURNAL OF SAFETY SCIENCE AND TECHNOLOGY,2022,18(12):75.[doi:10.11731/j.issn.1673-193x.2022.01.012]

备注/Memo

备注/Memo:
收稿日期: 2020-07-18
* 基金项目: 国家重点研发计划项目(2018YFC0807900);陕西省创新能力支撑计划项目(2018PT-33)
作者简介: 陈晓坤,博士,教授,主要研究方向为电气火灾物证鉴定与职业危害防治等。
通信作者: 王伟峰,博士,副教授,主要研究方向为电气火灾物证鉴定及煤火灾害监测预警技术等。
更新日期/Last Update: 2021-01-08